What was found
FAULT - DEBONDED SKIN , LOWER FACE OF LT WING T/E OTBD FLAP WEDGE LOWER SKIN , WS 663. IAW SRM 57-53-01-2R-1 REFER TO SRM 51-70-06-0G-0 REV. 55 PERFORM REPAIR AS BELOW STEP : 1.REMOVE THE DISBOND MATERIALS AND CLEAN. MEASURE THE DAMAGE SIZE AND LOCATION ( DIA : 1", 9" FROM LOWER EDGE AND 130" FROM INBD EDGE ). BONDED THE REPAIR PLIES WITH RESIN CURED AT 150°F FOR 180 MINUTES WITH MINIMUM VACUUM OF 22 IN/HG. CONDITION CHECK IS SATISFACTORY.