What was found
R/H FS 280 BULKHEAD FLOOR SUPPORT POST IS CORRODED AT LOWER END OF RBL 11.16 - UPON FURTHER INVESTIGATION, FOUND CORROSION ON FLOOR SUPPORT POST AT LOWER END TO BE .046 DEEP. FLOOR POST IS OUT FO REPAIRABLE LIMITS IAW CRJ 900 SRM 53-00-00-101-001-A01. REMOVED UNSERVICEABLE FS 280 BULKHEAD R/H FLOOR PAST AT RBL 11.16 IAW CRJ 900 SRM 51-40-11-001-001-A01, 51-42-06-001-001-A01, AND 51-42-21-001-001-A01. ORIGINAL POST THICKNESS WAS .080 AND REMAINING WAS .034.