What was found
AFT CARGO COMPARTMENT LH TRANSITION ANGLE UPPER SURFACE HAS CORROSION AROUND NUT PLATE HOLES. FROM STA 727G TO STA 727H. / [01] STEPPED UP PILOT HOLES PER SRM 51-40-05. INSTALLED 2 EA SPLICE PLATES PER SRM 51-40-02;[02] AFT CARGO COMPARTMENT DAMAGE ON LT SIDEPLATE TRANSITION ANGLE UPPER SURFACE FORM STA 727G TO STA 727H; LBL 24; WAS FOUND TO BE OUT OF ALLOWABLE LIMITS IAW SRM 53-00-53-1A-2.;[03] REMOVED AFT CARGO COMPARTMENT LEFT ZEE CHANNEL SIDEPLATE FORM STA 727F+10 TO STA 807+10; LBL 24; WL 156 IAW SRM 53-00-53-2R-5.;[04] FABRICATED ZEE CHANNEL SIDEPLATE REPAIR PARTS IAW SRM 53-00-53-2R-5.;[05] VERIFIED 4. JOHN PRAMUK (TECHNICIAN); 24-JUN-2022 14:28 UTC <BR>FABRICATED ZEE CHANNEL SIDEPLATE REPAIR PARTS IAW SRM 53-00-53-2R-5.;[06] INSTALLED REPAIR PARTS IAW SRM 53-00-53-2R-5. CLICK BOND PUSH TEST TO BE ACCOMPLISHED ON STEP 1.;[14] CHANGED CORROSION MEASUREMENT ITEM 19 ONLY FROM LEVEL 3 TO LEVEL 2. ALL OTHER MEASUREMENTS WERE UNCHANGED BY ME. OUT OF 24 MEASUREMENTS I ENTERED ONLY LINE ITEM #19. <BR>ALSO INSPECTED 12. PEDRO ALBA (TECHNICIAN); 27-JUN-2022 08:38 UTC<BR>R&R TRANSITION FITTING PER SRM 53-00-53-2R-5. RII;