What was found
PANEL 194CL HAS SEVERAL FASTENERS HOLE ELONGATED.<[01] REPAIRED DAMAGE FASTENERS HOLES AS MARKED WITH A PERMANENT REPAIR AS PER B737SRM 51-70-04-2R-9 .MATERIALS USED PO#2008859 AND PO#1738579;[02] PERFORMED TAP TEST INSPECTION ON REPAIRED AREAS ;FOUND NO DELAMINATION AS PER B737 NDT 51-05-01 SECTION 5.;[03] REPAIRED DAMAGE FASTENERS HOLES AS MARKED WITH A PERMANENT REPAIR AS PER B737SRM 51-70-04-2R-9 .MATERIALS USED PO#2008859 AND PO#1738579.PERFORMED TAP TEST INSPECTION ON REPAIRED AREAS ;FOUND NO DELAMINATION;[04] C/W