JASC 5340
Service difficulty reports · 22,411
Reports filed under 5340 · Fuselage Main, Attach Fittings, newest first.
Query with SQL
duckdb -csv -c "SELECT sdr_id, difficulty_date, n_number, aircraft_make, aircraft_model, part_name, part_condition, jasc_code, discrepancy FROM 'https://openairdocs.org/data/latest/faa_service_difficulty_report.parquet' WHERE jasc_code = '5340' ORDER BY difficulty_date DESC"
Prints the whole list as CSV. It reads the release’s Parquet files over HTTPS, so there’s nothing to download first. Install DuckDB to run it.
SELECT sdr_id, difficulty_date, n_number, aircraft_make, aircraft_model, part_name, part_condition, jasc_code, discrepancy FROM 'https://openairdocs.org/data/latest/faa_service_difficulty_report.parquet' WHERE jasc_code = '5340' ORDER BY difficulty_date DESC
Run it at the DuckDB prompt, or in any tool that reads Parquet over HTTPS. More ways to query the release are on Use the data.
SDR USAA001535Attach Fitting · corrodedPIT - FOUND CORROSION 1 INCH BY 10 INCH AT STATION 1088-1104 RUNNING INBOARD OF S-5R SHELF. CORROSION LEVEL 1, TASK NR C53-701-01. (M)SDR UPS00833794Fitting · crackedINSPECTION TYPE:C123, IN THE AFT LOWER CARGO COMPT STA 1150 L35R, FITTING IS CRACKED. REMOVED FITTING IAW DC8 SRM 51-1-20D, LOCATED AND DRILLED NEW FITTING IAW DC8 SRM 51-1-24, FABRICATED DOUBLERS IAW DC8 SRM 53-2-0, ALODINED AND PRIMED IAW DC8 SRM 51-1-8, INSDR UPS00833955Fitting · corrodedINSPECTION TYPE:C123, FITTING CORRODED BEYOND LIMITS. REPLACED FITTING IAW DC8 SRM 51-1-20D.SDR UPS00833796Fitting · crackedINSPECTION TYPE:C123, AFT LOWER PIT TRANSVERSE FLOORBEAM END FITTING CRACKED BETWEEN BOLT HOLES FS 1160 BL 66R AT FWD UPPER CORNER OF C-PIT DOOR. REMOVED TRANSVERSE FLOORBEAM END FITTING IAW DC8 SRM 57-1-20D END FITTING FOUND TO BE CRACKED RCVD. ORDERED NEW SDR EISA20000175Fitting · crackedPERFORMED HFEC ON FWD LANDING GEAR DOOR HINGE FITTING FOUND CRACKS TOTAL OF 8 HOLES LT AND RT SIDE. REAMED ALL SIDES, CLEANED, SHOT PEENED FITTINGS, ALODINED, PRIMED AND INSTALLED IAW B727 SRM 51-10-2, SOPM 20-10-03 AND SB 727-32-0340.SDR UPS00833740Fitting · crackedINSPECTION TYPE:C123, STA 1690 LONG 26R END FITTING IS CRACKED. REMOVED AND REPLACED FITTING IAW DWG 4641326 AND SRM 51-1-20D, 51-3-0.SDR UPS00833721Fitting · crackedINSPECTION TYPE:C123, STA 1180 BATHTUB FITTING BETWEEN LONG 34R - 35R IS CRACKED. REMOVED AND REPLACED FITTING IAW DWG 3755843 AND SRM 53-2-0 FIG 2D.SDR SWAA001621Fitting · crackedDURING SCHEDULED 1/2D CHECK, FOUND BS 727 BULKHEAD VERTICAL BEAM UPPER FITTING CRACKED. REMOVED AND REPLACED FITTING PER SRM.SDR CALA0001342Floor Support · crackedINSPECTION FOUND A 6 INCH CRACK IN MID CARGO BAY FIBERGLASS FLOOR SUPPORT ANGLE AT STA 617, LONGERON 26R TO 27R. THE FLOOR SUPPORT ANGLE WAS REMOVED, REPAIRED WITH FIBERGLASS OVERLAY, AND REINSTALLED IAW SRM 51-70-1, FIGURE 4 AND 51-30-5.SDR L1GA200000265Attach Angle · crackedA 1 INCH CRACK AFT FUSELAGE ABOVE APU ENCLOSER STEP STRUCTURE. FABRICATED REPAIR ANGLE.SDR 00FDEA00595Attach Angle · crackedDURING ROUTINE INSP, ATTACH ANGLE AT BS 720F FROM STR 28L TO 28R FOUND CRACKED. REMOVED, REPLACED AND FAB PER IAW SRM 51-20-1 AND 51-30-2.SDR GAIA00575Fitting · crackedDISCREPANCY: DURING HEAVY CHECK FOUND: SEAT TRACK FITTING CRACKED AT STA 740 RBL24CORRECTIVE ACTION: REPAIRED IAW B727 SRM 53-10-8SDR USAA001453Mount · corrodedPIT - FOUND MOUNTS CORRODED .25 INCH IN FOUR PLACES, AFT LAV FORWARD MOUNTS. REMOVED AND REPLACED LEFT FORWARD MOUNTS PE SRM 51-40-00. CORROSION LEVEL 1, TASK NR C53-107-02. (M)SDR CALA0001274Attach Angle · crackedINSPECTION FOUND A .5 INCH CRACK IN VERTICAL STABILIZER TO FUSELAGE ATTACH ANGLE AT STA 1486, L3R. THE ATTACH ANGLE WAS REMOVED AND A NEW ANGLE WAS INSTALLED IAW SRM 53-05, FIGURE 23.SDR P2EA00244Fitting · misdrilledDURING C-CHECK, LOWER HOLE IN FITTING AT BS 695 BORED SLIGHTLY OFFSET. ENLARGED HOLE TO .9375 DIA AND INSTALLED BUSHING IAW MPP B737-VAG-00-53-010. (M)SDR TWAA0013307Attach Angle · crackedDURING CHECK-C MAINT, FOUND CHAIR TRACK ATTACH ANGLE CRACKED AT STA 927, RBL 22 AT WING SKIN. REMOVED CRACKED FLOOR SUPPORT ANGLE AT STA 927, RBL 22, NUMBER 3 CHAIR TRACK, AND INSTALLED NEW PER DOUGLAS INSTALLATION DRAWING 3925819.SDR CALA0001264Fitting · corrodedINSPECTION FOUND LT SIDEWALL LOWER ATTACH FITTING CORRODED AT STA 200. A NEW FITTING WAS INSTALLED IAW SRM 51-30.SDR UPS00833615Fitting · crackedINSPECTION TYPE:C2, AFT PIT L25 LT STA 1040 - 1060 SPLICE HAS 2'' CRACKED (MKD) DOT J974. REMOVED FILLET PANEL IAW DC8 SRM 51-3-0. REMOVED FITTING IAW DC8 SRM 51-1-21, DRILLED AND LOCATED FITTING IAW DC8 SRM 51-1-24, INSTALLED FITTING IAW DC8 SRM 51-1-20D, ISDR RRXA003137Fitting · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE FITTING FOR FRAME TO FUSELAGE FWD SIDE OF FITTING AT STA Y=880 AND L21R-L22R, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. RECEIVED PART AND INSTALLED IAWSDR UPS00833614Attach Angle · crackedINSPECTION TYPE:C2, FUSELAGE AFT RT LOWER FILLET PANEL ATTACH ANGLE CRACKED STA 1080 & L30R. REMOVED PART FROM AIRCRAFT IAW DC8 SRM 53-2-0, BLENDED WITHIN ALLOWABLE LIMITS. ALODINED AND PRIMED ATTACH ANGLE IAW DC8 SRM 51-1-8. INSTALLED ATTACH ANGLE IAW DC8 SDR AALA20001398Fitting · corrodedTUL - FOUND CORROSION ON FITTING AT AFT CARGO DOOR OPENING LOWER AFT CORNER AT L28R STATION 1212. INSTALLED NEW FITTING AT AFT CARGO DOOR OPENING LOWER AFT CORNER AT L28R STATION 1212. AS PER MM 20-10-15-2 AND SRM 51-10-4. (M)SDR AALA20001397Fitting · corrodedTUL - FOUND CORROSION ON FITTING AT AFT CARGO DOOR OPENING LOWER FORWARD CORNER AT LONGERON 28R, STATION 1155. INSTALLED NEW FITTING ON LOWER FORWARD CORNER OF AFT CARGO DOOR OPENING AT STATION1155 L28R PER MM 20-10-15-2. (M)SDR C2XA00IA291Attach Angle · corrodedFOUND FLIGHT DECK TO CAPTAIN FLOOR ATTACH ANGLE HAS SURFACE CORROSION PITTING. REMOVED AND REPLACED ATTACH ANGLE IAW EMB-120 SRM 51-40-02. (M)SDR L1GA200000198Attach Fitting · crackedA 3 INCH CRACK AT FS 680 BL 45 RT ABOVE CENTER WING. REPLACED WITH IDENTICAL PART, MAJOR REPAIR.SDR RRXA003783Attach Angle · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE LONGERON ATTACH ANGLE AT STA 1180 AND L28L, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AND PRIMED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED REPAIR IAW DC-8 SRM 53-2-0 FISDR TWAA0013203Fitting · corrodedDURING CHECK-C MAINT, THE SILL AREA IN AFT CABIN HAD CORROSION ON MEMBRANE WIDTH OF DOOR, INTERGRANNULAR BELOW AFT GIRT BAR MOUNT FITTING, STA 1136L TO 1193L, LBL 50 TO LBL 54. REMOVED LIGHT TO MODERATE CORROSION. TREATED, PRIMED AND PAINTED PER SRM 51-10-03SDR QXEA0002069Attach Angle · crackedPDX- REAR PRESSURE BULKHEAD BL 1250R HAS TWO SHREADED RIVETS AND THREE CRACKS ON VERTICAL ATTACH ANGLE BETWEEN BEAMS 6 AND 7. REPAIRED IAW FOKKER SRM 51-31-01, 51-10-05 AND 51-11-04.SDR RRXA003782Attach Angle · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE LWR CARGO PIT CEILING SUPPORT AT STA 1390, X=+41 TO -41, Z+-6, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. /////CORRECTIVE ACTION///// REMOVED DAMAGE, TREATED AND PRIMED AREA IAW DC-8 SRM 51-1-8. FABRICSDR RRXA003780Attach Angle · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE AFT LWR CARGO COMPT FLOOR ATTACH STRAP AT STA 1390 AND L35L TO L35R, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. /////CORRECTIVE ACTION///// REMOVED DAMAGE, TREATED AND PRIMED AREA IAW DC-8 SRM 51-1-8. SDR AALA20001264Fitting · crackedTUL - FOUND CRACK INDICATION IN BOTTOM OF C HOLE MOST INBOARD FORWARD FLANGE OF AFT BULKHEAD FITTING. ACCOMPLISHED BY WORKCARDS ECO ESO DR 549404-DR549402 P-4233, 4234, 4439, 4450, 4483, 4932. ECO-45594B, ESO 8783 UPPER SPAR REWORKED, DC10-5485 ESO 7349 D-1-SDR RRXA003775Angle · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE LOWER ANGLE AT STA 857 X=0 TO+25 Z+-21, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AND PRIMED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED FILLETS IAW DC-8 SRM 53-2-0 FIG 1SDR UPS00233557Fitting · corrodedINSPECTION TYPE:SI, MAIN DECK FLOOR WEB FITTING CORRODED (C53-224-01.00-03) BETWEEN LEFT CREASE BEAM AND DITCHING PAN, FWD OF BS 1183 BULKHEAD BS 1180 LBL 65, WL 208. REMOVED AND REPLACED FLOOR WEB FITTING IAW SRM 51-30-05, 53-10-01, 51-10-06.SDR UPS00833467Fitting · crackedINSPECTION TYPE:C123, STA 798 LBL 50 ANGLE IS CRACKED UPPER SIDE CENTER FUEL TANK. REMOVED AND REPLACED ANGLE IAW DWG 3643112, AND SRM 51-1-20D.SDR UPS00833574Fitting · corrodedINSPECTION TYPE:C123, STA 70 FRAME TO CUSP FITTING IS CORRODED BEYOND LIMITS. REMOVED, FABRICATED AND REPLACED FITTING IAW DWG 3610130 AND DH SK 806-478 AND SRM 51-1-21, 51-3-0.SDR UPS00833495Fitting · crackedINSPECTION TYPE:C123, STA 300 LONG 27L BANANA FITTING IS CRACKED. REMOVED AND REPLACED FITTING IAW DWG 3754041 AND SRM 51-1-20D, 51-1-21, 53-2-0 FIG 1D.SDR CALA0001122Fitting · corrodedINSPECTION FOUND FORWARD AND AFT GIRT BAR FITTINGS CORRODED AT STA 160 AND 200, RBL 54. NEW FITTINGS WERE INSTALLED IAW SRM 51-10-4 AND 51-30-1.SDR UPS00833560Fitting · crackedINSPECTION TYPE:C123, STA 680 LONG 8L END FITTING IS CRACKED. REMOVED AND REPLACED FITTING IAW DWG 3779762 AND SRM 51-1-20D, 51-1-21, 51-1-23.SDR UPS00833532Fitting · crackedINSPECTION TYPE:C123, STA 220 - 240 LONG 18R SPLICE FITTING IS CRACKED. REMOVED, FABRICATED AND REPLACED FITTING IAW DWG 4651908, 8110-3 APPROVED DH SK 806-498 AND SRM 51-1-20D.SDR UPS00833530Fitting · crackedINSPECTION TYPE:C123, STA 834 LONG 13L ATTACH FITTING IS CRACKED. REMOVED, FABRICATED AND REPLACED FITTING IAW DWG 3779874 AND SRM 51-1-20D.SDR UPS00833440Fitting · crackedINSPECTION TYPE:C123, STATION 1170 RT UPPER CUSP FITTING IS CRACKED. REMOVED AND REPLACED FITTING IAW DWG 3754918 AND SRM 51-1-20D.SDR MWEA00582Attach Angle · crackedSECONDARY ATTACH ANGLES CRACKED AT STATION 83 LEFT AND RIGHT SIDE. FABRICATED AND INSTALLED DOUBLERS AND FILLERS.SDR UPS00433400Fitting · crackedINSPECTION TYPE:SP, L3 DOOR, STOP FITTING NR 4 IS CRACKED. REMOVED AND REPLACED FITTING IAW DWG 015U0579 AND SRM 51-30-2.SDR CALA0001100Attach Angle · corrodedINSPECTION FOUND AFT CARGO THRESHOLD ATTACH ANGLE CORRODED AT FS 1211, LONGERON 26R TO 27R. THE ATTACH ANGLE WAS REMOVED AND REPLACED IAW SRM 51-30-1 AND 51-10-4.SDR RRXA003694Attach Angle · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE OVERHEAD ANGLE SUPPORT AFT SIDE FOR BAGG LINER AT STA 1320, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED REPAIR IAW DC-8 SRM 53-2SDR RRXA003686Angle · corrodedDURING A MAINTENANCE VISIT FOUND CORROSION DAMAGE TO THE OVERHEAD ANGLE SUPPORT FOR BAGGAGE LINER AT STA 1320, DAMAGE EXCEEDED LIMITATIONS IAW DC-8 SRM. REMOVED DAMAGE, TREATED AREA IAW DC-8 SRM 51-1-8. FABRICATED AND INSTALLED REPAIR IAW DC-8 SRM 53-2-0. (SDR AALA20001191Support Bracket · corrodedTUL - FOUND GALLEY SUPPORT NR/NR 4 RIGHT BETWEEN FRAME 78 AND FRAME 79 CORRODED. REPAIRED GALLEY SUPPORT NR 4 RIGHT BETWEEN FRAME 78 AND 79 PER ESO 30595 DATED 07-17-00. (M)SDR DLL14001339Attach Fitting · crackedTHE ATTACH FITTING COMMON TO THE R4 DOOR NR 1 DOOR STOP INTERCOSTAL AND THE AFT PRESSURE BULKHEAD WAS FOUND CRACKED. THE CRACK IS TYPICAL OF LAC S/B 093-53-270. THE ADJACENT FITTINGS WERE FOUND UNDAMAGED. THE CRACKED FITTING WAS AUTHORIZED FOR CONTINUEDSDR DLL14001338Attach Fitting · crackedTHE ATTACH FITTING COMMON TO THE L4 DOOR NR 1 DOOR STOP INTERCOSTAL AND THE AFT PRESSURE BULKHEAD WAS FOUND CRACKED. THE CRACK IS TYPICAL OF LAC S/B 093-53-270. THE ADJACENT FITTINGS WERE FOUND UNDAMAGED. THE CRACKED FITTING WAS AUTHORIZED FOR CONTINUEDSDR SIMA2073Intercostal · corrodedSAW - DURING CPCP-2 INSPECTION, MAINTENANCE FOUND THE SERVICE DOOR SILL PLATE INTERCOSTAL BETWEEN FRAMES 39 AND 40 CORRODED. MAINTENANCE REMOVED AND REPLCCED THE INTERCOSTAL IAW ATR SRM 51-25-01. AIRCRAFT WAS RETURNED TO SERVICE. (M)SDR QXEA0001841Attach Angle · crackedPDX- LEFT HAND INBOARD SEAT TRACK TO FRAME 9305B INBOARD ATTACH BRACKET IS CRACKED AT UPPER RADIUS. REPAIRED IAW FOKKER SRM 51-31-01, PAGE 13.
Back to JASC 5340