JASC 5753
Service difficulty reports · 31,521
Reports filed under 5753 · Trailing Edge Flaps, newest first.
Query with SQL
duckdb -csv -c "SELECT sdr_id, difficulty_date, n_number, aircraft_make, aircraft_model, part_name, part_condition, jasc_code, discrepancy FROM 'https://openairdocs.org/data/latest/faa_service_difficulty_report.parquet' WHERE jasc_code = '5753' ORDER BY difficulty_date DESC"
Prints the whole list as CSV. It reads the release’s Parquet files over HTTPS, so there’s nothing to download first. Install DuckDB to run it.
SELECT sdr_id, difficulty_date, n_number, aircraft_make, aircraft_model, part_name, part_condition, jasc_code, discrepancy FROM 'https://openairdocs.org/data/latest/faa_service_difficulty_report.parquet' WHERE jasc_code = '5753' ORDER BY difficulty_date DESC
Run it at the DuckDB prompt, or in any tool that reads Parquet over HTTPS. More ways to query the release are on Use the data.
SDR UPS99229557Track · corrodedINSPECTION TYPE:SI, CORROSION (C57-581-06.00-04) ON NR 7 FLAP TRACK AT FWD ATTACH LUG AND INSIDE BARREL NUT HOLE. REPAIRED PER ER 99-5243.SDR UPS99229556Fitting · corrodedINSPECTION TYPE:SI, CORROSION (C57-581-06.00-04) ON NR 5 FLAP TRACK FWD ATTACH FITTING. REMOVED AND REPLACED SUPPORT ASSY.SDR UPS99229555Track · corrodedINSPECTION TYPE:SI, CORROSION (C57-581-06.00-04) ON NR 7 FLAP TRACK AT FWD ATTACH LUG AND INSIDE BARREL NUT HOLE. REPAIRED ON CUSTOMER ID 888950.SDR DHL9970135DSkin · delaminatedAT D-CHECK, RT WING O/B FLAPS AFT FLAP UPPER SURFACE 12 INCHES FROM I/B EDGE SECTION DELAMINATED. INSTALLED OVERLAY REPAIR PER SRM 51-40-8, 8 X 6.SDR DHL9970134DSkin · delaminatedAT D-CHECK, RT WING O/B FLAPS AFT UPPER SURFACE 73 INCHES FROM I/B EDGE SECTION DELAMINATED. INSTALLED OVERLAY REPAIR PER SRM 51-40-9, 14 X 6.SDR DHL9970133DSkin · delaminatedAT D-CHECK, RT WING O/B FLAPS AFT FLAP UPPER SURFACE 134 FROM I/B EDGE AREA DELAMINATED. INSTALLED FIBREGLASS OVERLAY REPAIR PER SRM 51-40-8, 4 X 9.SDR CALA9900321Skin · crackedINSPECTION FOUND A 1 CRACK IN RT WING OUTBOARD FLAP SKIN. THE SKIN WAS REPLACED IAW DOUGLAS DRAWING ARC1653.SDR UPS99229447Casting · crackedINSPECTION TYPE:C+SI, CRACK ON OUTBOARD FLAP CONTROL VALVE SUPPORT CASTING IN ROOF OF RT MLG WHEEL WELL. REPLACED HOUSING IAW MM 27-51-51 AND OHM 20-50-02.SDR ABXA9900263Vane · delaminatedDURING C-CHECK, FOUND LEFT INBOARD FIXED VANE DELAMINATED. REPLACED LEFT INBOARD FIXED VANE IAW DC9 MM 27-51-3.SDR SWAA990551Skin · puncturedDURING SCHEDULED A1 CHECK, FOUND LEFT I/B FOREFLAP HAS .75 INCH PUNCTURE AT BOTTOM SIDE, 36 INCHES FROM I/B END. REPAIRED PER SWA RA NR 1-357-0655 AND SRM.SDR DL72W990919Spar · crackedAFT SPAR CRACKED 22 FROM I/B END OF FLAP, THIS DAMAGED WAS REPAIRED PER MM 57-52-0 FIG 802 ON SHOP N/R 011630 LOCATED SHOP ORDER 709228.SDR DL72W990918Spar · damagedTEMP SPLICE AFT SPAR AT 57 AND 46 FROM I/B END OF FLAP. THIS DAMAGE WAS REPAIRED PER MM 57-52-0 FIG 802 ON SHOP N/R 011626, LISTED ON SHOP ORDER 709228.SDR DL72W990814Angle · crackedDURING SHOP INSPECTION, THE AFT LOWER CLOSEOUT SPAR ANGLE WAS FOUND CRACKED 2 PLACES 35 FROM IB END OF FLAP. A NEW SECTION OF SPAR ANGLE WAS DRILLED UP AND INSTALLED PER MM 57-52-01, FIG. 802.SDR DL72K990614Spar · misdrilledDURING SHOP VISIT AND ACCOMPLISHMENT OF EO 4-58705-3AD, MTC UNABLE TO INSTALL REQUIRED COLLAR FOR ONE OF THE UPPER SPAR-TO-UPPER SKIN ATTACH FASTENERS DUE TO PROXIMITY TO SPAR RADIUS. AUTHORIZED USE OF RADIUS BLOCK AND MINI NUT.SDR UPS99229076Rib · crackedINSPECTION TYPE-C RT WING I/B FOREFLAP TRACK SUPPORT I/B RIB ASSY IS CRACKED. REMOVED AND REPLACED RIB ASSY PER SRM 51-30-02.SDR CALA9900281Skin · crackedINSPECTION FOUND A 1.25 INCH CRACK IN RT O/B FOREFLAP LEADING EDGE. THE CRACK WAS STOP DRILLED. A DOUBLER WAS INSTALLED IAW SRM 57-50-4 AND 51-30-2, PAGE 7.SDR CALA9900279Skin · tornINSPECTION FOUND RT I/B FOREFLAP INBOARD MOST END UPPER LEADING EDGE SKIN TORN FORWARD OF SPRING DOOR. THE FOREFLAP WAS REMOVED AND REPLACED IAW MM 27-51-3.SDR CALA9900278Skin · crackedINSPECTION FOUND A .3125 INCH CRACK AT RT I/B MIDFLAP LOWER TRAILING EDGE. THE CRACK WAS STOP DRILLED. A DOUBLER WAS INSTALLED IAW SRM 51-40-2 AND 51-30-2.SDR CALA9900277Skin · disbondedINSPECTION FOUND LT TRAILING EDGE I/B FOREFLAP DISBONDED AT UPPER AND LOWER SURFACE. THE FOREFLAP WAS REMOVED AND REPLACED IAW MM 27-51-4.SDR CALA9900264Fairing · delaminatedINSPECTION FOUND LT WING FLAP FAIRING 574CB FORWARD EDGE OUTER SKIN PLIES DELAMINATING. THE FAIRING WAS REMOVED, REPAIRED IAW SRM 51-70-04, AND REFITTED IAW MM 27-51-31.SDR CALA9900263Fairing · delaminatedINSPECTION FOUND FLAP FAIRING 572HB FORWARD EDGE OUTER SKIN PLIES DELAMINATED. THE FLAP FAIRING WAS REMOVED, REPAIRED IAW SRM 51-70-03, AND REFITTED IAW MM 27-51-30.SDR CALA9900259Skin · gougedINSPECTION FOUND LT WING O/B UPPER SURFACE INBOARD FLAP PANEL GOUGED BY SPOILER. THE PANEL WAS REMOVED AND REPAIRED IAW ECRA 5753-01061 AND REFITTED IAW MM 57-51-00.SDR CALA9900255Panel · gougedINSPECTION FOUND RT WING O/B FLAP UPPER SURFACE INBOARD PANEL GOUGED BY SPOILER. THE PANEL WAS REPAIRED IAW ECRA 5753-01061 AND REFITTED IAW MM 57-51-00.SDR DL72S990616Flap Track · corrodedDURING OUTSIDE REPAIR, OVERHAUL PER CMM AND MOD PER SB 727-57-0178, TYPICAL CORROSION WAS FOUND TO THE FWD ATTACH LUGS AND THE MLG BEAM AND SPOILER BEAM ATTACH PADS AND HOLES. AUTHORIZED BUSHING REPAIR FOR FWD ATTACH LUG AND OVERSIZED SPOILER BEAM ATTACH HSDR DL72S990615Flap Track · corrodedDURING OUTSIDE REPAIR OF COMPONENT AND OVERHAUL PER CMM AND MOD PER SB 727-57-0178, TYPICAL CORROSION WAS FOUND ON THE MLG BEAM AND SPOILER BEAM ATTACH PAD AND HOLES. AUTHORIZED OVERSIZED FASTENERS, BUSHING REPAIR AND LEAVING THE OVERSIZED MLG BEAM ATTACH HOLSDR CKSA99012Skin · groovedDURING ACCOMPLISHMENT OF C-CHECK, FOUND RT WING NR 2 FLAP VANE LEADING EDGE IS GROOVED 20 I/B FROM VANE O/B END. CUT OUT DAMAGED AREA AS REQUIRED PER SRM 51-53-00 FIG 812. FABRICATED REPAIR DOUBLERS, TRIMMED, DEBUR AND REPROTECTED IAW SRM 51-21-00. INSTALLESDR USAA990251Skin · corrodedPIT - DURING C5 CHECK, FOUND 1 INCH LONG, 1 INCH WIDE, .011 DENT AND 1 INCH LONG, 1 INCH WIDE, .009 DEEP DENT AT RIGHT WING INBOARD FLAP, AFT SIDE, MIDDLE OF TOP CENTER SKIN PANEL. CORROSION LEVEL 1. CLEANED AND TREATED CORROSION PER SRM CHAP 51. (M)SDR ABXA9900179Vane · delaminatedRIGHT WING FLAP CENTER FIXED VANE DELAMINATED ON LOWER SURFACE AT INBOARD END. REPLACED VANE IAW DC9 MM 27-51-3.SDR MZZA99075Plate · corrodedTNN - DURING D-CHECK INSPECTION ON AIRCRAFT AT AIR ASIA, A 1 INCH DIAMETER CORROSION WAS FOUND ON RIGHT INBOARD MIDFLAP INNER SPLICE PLATE AT WBL 242. THE CORROSION WAS REMOVED AND REPAIRED PER SRM 51-30-02, 51-10-02. (M)SDR CALA9900237Skin · delaminatedINSPECTION FOUND RT WING OUTBOARD AFT FLAP LOWER SURFACE DELAMINATED AND DENTED O/B OF INBOARD TRACK. REPAIRED IAW SRM 57-53-01, PAGE 205 AND SRM 51-70-17, PARAGRAPH 3A.SDR SWIA971429Skin · dirtyAIRCRAFT NEEDS LEFT AILERON TRIM WHEN FLAPS SET TO 45 DEGREES. DISCOVERED LEADING EDGE OF FLAP HAD RIDGE OF PAINT BUILD-UP FROM RECENT AIRCRAFT RE-PAINTING. RE-SURFACED LEADING EDGE OF FLAP IAW SERVICE LETTER RJ-SL-27-022 DATED 8/28/96.SDR MZZA99081Track · rustedTNN - DURING D-CHECK INSPECTION ON AIRCRAFT AT AIR ASIA, RUST WAS FOUND ON NR 4 FLAP TRACK FORWARD MOUNTING PAD A UPPER SURFACE AND HOLES. THE RUSTED TRACK, P/N 65-19269-20 WAS REMOVED AND REPLACED WITH P/N 65-19269-13 PER B727 MM 27-51-31 AND OPERATIONAL CHESDR MZZA99076Rear Spar · corrodedTNN - DURING D-CHECK INSPECTION ON AIRCRAFT AT AIR ASIA, A 3 INCH BY 5 INCH AREA CORROSION WAS FOUND ON RIGHT OUTBOARD MIDFLAP REAR SPAR LOWER CHORD FORWARD FLANGE AT WBL 431. THE CORROSION WAS REMOVED AND REPAIRED PER ECRA 5750-03184 DATED ON APR 6, 1999. (SDR MZZA99074Angle · crackedTNN - DURING D-CHECK INSPECTION ON AIRCRAFT AT AIR ASIA, A .25 INCH LONG CRACK WAS FUOND ON RIGHT INBOARD MIDFLAP T/E LOWER CLOSURE ANGLE AT WBL 108. THE CRACKED AREA WAS CUT OFF AND REPAIRED PER SRM 51-40-04, 51-30-02. (M)SDR DHL9980755CSkin · wornAT C CHECK, LT O/B FLAP L/E I/B LOWER SECTION HAS FASTENER HOLES ELONGATED. FABRICATED DOUBLER PER SRM 57-2-0, 3.375 BY 2.5. N/R 267SDR DHL9980754CSkin · dentedLEFT O/B FLAP AT T/E LOWER AREA O/B SECTION HAS DENT DAMAGE ON SURFACE STA XW 456.5. REMOVED DAMAGED SECTION. FABRICATED NEW SECTION AND INSTALLED PER SRM 51-1-21, 40 BY 10. N/R 261SDR DHL9980742Bracket · brokenAT C-CHECK, LT WING FLAP VANE NR 4 O/B ATTACHING BRACKET AT L/E BROKEN. REMOVED AND REPLACED O/B ATTACH BRACKET PER MM 27-51-14.SDR DHL9980741CPanel · crackedAT C-CHECK, LT WING T/E AREA INNER WING FLAP MECHANISM SUPPORT FITTING HAS UPPER PANEL WITH CRACK ON SURFACE. STOP DRILLED END OF CRACK, FABRICATED DOUBLER PER SRM 51-1-8 AND INSTALLED PER 51-1-21, 6.375 X 3.5.SDR DHL9980740CAngle · crackedAT C-CHECK, LT O/B FLAP EXHAUST GATE CUTOUT AT I/B SECTION INTERIOR OF T/E HAS CRACK ON FORMED ANGLE. REMOVED DAMAGED T/E SECTION ON EXHAUST GATE CUTOUT, FABRICATED NEW SECTION AND NEW ANGLE AND INSTALLED PER SRM 51-1-20B, 8.5 X 26 AND 55 X 26.SDR TWAA9904008Skin · damagedDURING CHECK-C MAINT, FOUND ON LT WING, THE O/B TRAILING EDGE FLAP WITH A .25 IN HOLE AT I/B END OF LOWER SURFACE. INSTALLED A 2 IN BY 2 IN WET LAY-UP PER SRM 51-70-06.SDR TWAA9904006Skin · damagedDURING CHECK-C MAINT, FOUND LT WING TRAILING EDGE AFT FLAP OF THE I/B FLAP WITH A HOLE 28 IN I/B OF O/B EDGE, 9 IN AFT OF LEADING EDGE. INSTALLED HOT BOND REPAIR PER SRM 57-53-01, 350 DEG CURE PERMANENT REPAIR, AND PAINTED HOT BOND REPAIR.SDR DHL9980769CVane · delaminatedAT C CHECK, LEFT WING NR 4 FLAP VANE IS DELAMINATED. REMOVED AND REPLACED VANE PER MM 27-51-14. N/R 42SDR DHL9980767CVane · delaminatedAT C CHECK, RT FLAP VANE FLAP PANEL NR 3 DELAMINATED. REMOVED VANE AND REPAIRED AND REINSTALLED PER MM 27-50-0..SDR DHL9974121CSkin · delaminatedAT C CHECK, RT WING O/B AFT FLAP T/E DELAMINATED. INSTALLED FIBERGLASS OVERLAY REPAIR PER SRM 51-40-8, 10 BY 5, N/R 2898.SDR AU990990Bracket · cracked(AUS) FLAP ACTUATOR SUPPORT BRACKETS P/N 261114-6 (FORWARD) AND P/N 261114-7 (AFT) CRACKED AND DISTORTED. SUBMITTER SUSPECTED CAUSED BY MISRIGGING OF THE FLAP POSITION SWITCH ASSEMBLY.SDR TWAA9903606Bolts · rustedDURING OP 15 MAINT CHECK, FOUND 4 I/B AFT FLAP CASTING ATTACH BOLTS ON REAR SPAR EMITTING RUST. REPLACED STUDS AND HINGE FITTING PER MM 57-40-0 AND 27-51-1.SDR QXEA9900427Track · corrodedPDX - NR 3 RIGHT-HAND FLAP TRACK HAS LIGHT TO MODERATE SURFACE PITTING ON LOWER TRACK TOP SURFACE IN ROLLER PATH AND UPPER TRACK BOTTOM SURFACE IN ROLLER PATH. REPAIRED IAW HORIZON AIR EA 9-57-406.SDR DHL9974157CSkin · delaminatedAT C CHECK, LEFT WING I/B FORE FLAP DELAMIANTED IN TWO AREAS AT CENTER SECTION. INSTALLED BONDED REPAIR PER SRM 57-40-6, 10 BY 8 AND 13 BY 17 FT, N/R 1457.SDR GAIA99039Skin · damagedDURING C-CHECK, DAMAGE WAS FOUND ALONG THE OUTBOARD MID-FLAP LOWER SKIN. THE PART HAS A MILLED OPENING FOR AN ACCESS PANEL. THE NUTPLATE HOLES WERE DAMAGED. A REPAIR DOUBLER WAS FABRICATED FROM 2024-T3 BY .0100 INCH CLAD ALUMINUM. THE REPAIR WAS ACCOMPLISHSDR DHL9974158CSkin · damagedAT C CHECK, L/T WING I/B MID FLAP LOWER SURFACE LOWER SKIN PANEL HAS A CRACK JUST O/B OF NR 4 TRACK FAIRING. TRIMMED OUT DAMAGED, INSTALLED REPAIR AT LEFT WING MID FLAP PER SRM 57-50-4, 4 BY 22.5, N/R 1452.
Back to JASC 5753